Atomic Layer Deposition of SnO2-Coated Anodic One-Dimensional TiO(2 )Nanotube Layers for Low Concentration NO2 Sensing

ACS APPL MATER INTER

NG, S.; PRÁŠEK, J.; ZAZPE, R.; PYTLÍČEK, Z.; SPOTZ, Z.; RODRIGUEZ-PEREIRA, J.; MICHALIČKA, J.; PŘIKRYL, J.; KRBAL, M.; SOPHA, H.; HUBÁLEK, J.; MACÁK, J., 2020: Atomic Layer Deposition of SnO2-Coated Anodic One-Dimensional TiO(2 )Nanotube Layers for Low Concentration NO2 Sensing. ACS APPL MATER INTER , p. 33386 - 11, doi: 10.1021/acsami.0c07791; FULL TEXT