Friak, M; Bursikova, V; Pizurova, N; Pavlu, J; Jiraskova, Y; Homola, V; Mihalikova, I; Slavik, A; Holec, D; Vsianska, M; Koutna, N; Fikar, J; Janickovic, D; Sob, M; Neugebauer, J, 2019: Elasticity of Phases in Fe-Al-Ti Superalloys: Impact of Atomic Order and Anti-Phase Boundaries. CRYSTALS 9(6), doi: 10.3390/cryst9060299